Hardness82-84 HDTensile Strength35-45 MPaElongation at Break35-40%Izod Impact Strength212 J/m -
11th AnniversaryNozzle≥0.4 mmDry before PrintingRecommendedPrinting Temp.210-240 ℃Hotbed Temp.55-65 ℃ -
Nozzle≥0.2 mmDry before PrintingRequiredPrinting Temp.230-250 ℃Hotbed Temp.60-70 ℃ -
11th AnniversaryFully-Enclosed PrintingRecommendedNozzle≥0.4mmPrinting Temp.255-275 ℃Hotbed Temp.80-100 ℃